AI detection evidence

crack 89%Linear crack along panel joint, water staining observed after rainfall.
Engineering review workflow
Reviewing engineer
Eng. Chan Vibol
Recommendation
Immediate sealing and re-coating; verify with water test after repair.
Finding record
- Crack ID
- CR-009
- Zone
- Z-A2 — Terminal Roof A2
- Width
- 2.9 mm
- Length
- 3.6 m
- AI confidence
- 89%
- Detected
- 2026-03-01
- Method
- Drone RGB
- Severity
- High
- Status
- Verified
Linked maintenance
No maintenance task created yet for this finding.

Example after-repair evidence photo.